Uretyco
Make it now
Polypropylene (PP)

Polypropylene (PP)

Plastics
PPPolypropyleneInjection MoldingCommodity

Polypropylene (PP) reference: homopolymer vs. copolymer properties, injection-molding design rules, living hinges, FDM printing limits, decoration, cost drivers, and comparison with HDPE, ABS, POM and PA12.

Polypropylene (PP) is a semi-crystalline polyolefin and one of the cheapest and lightest molding plastics, with a density of about 0.90 g/cm³. It resists most acids, alkalis and aqueous chemicals, absorbs almost no water, and survives a very large number of flex cycles in a thin section, which makes it the standard material for living hinges. It comes as homopolymer (stiffer, more heat-resistant), random copolymer (clearer, more flexible) and impact copolymer (tough down to sub-zero temperatures).

Choose it for injection-molded parts in volume: closures, containers, clips, housings and labware where chemical resistance, low weight and cost matter more than stiffness or precision. For tight-tolerance, load-bearing or hot parts, its high mold shrinkage, low stiffness and creep make ABS, POM or PA better choices.

Mechanical and physical properties

PropertyTypical valueNotes
Density0.90–0.91 g/cm³Floats in water; more parts per kilogram of resin.
Tensile strength (yield)≈ 30–40 MPaHomopolymer; copolymers ≈ 20–30 MPa.
Elongation at break> 100%Ductile at room temperature; often several hundred percent, grade-dependent.
Tensile modulus≈ 1.3–1.8 GPaHomopolymer; copolymers ≈ 0.9–1.3 GPa. ABS is ≈ 2.0–2.5 GPa.
Notched impact (Charpy, 23 °C)≈ 3–6 kJ/m²Homopolymer, brittle near 0 °C; impact copolymers ≈ 8–50 kJ/m² and stay tough in the cold.
Heat deflection temperature≈ 75–110 °CAt 0.45 MPa; only ≈ 50–60 °C at 1.8 MPa. Homopolymer at the upper end.
Melting point≈ 160–165 °CHomopolymer; random copolymers melt lower (≈ 140–150 °C).
Continuous service temperature≈ 80–100 °CUnloaded, heat-stabilized grades; creep limits loaded use.
Mold shrinkage≈ 1.0–2.5%Varies with grade, wall thickness and flow direction; fillers reduce it.
Water absorption (24 h)< 0.1%Dimensions stay stable in humidity.
Thermal expansion≈ 100–150 µm/m·KAbout five times aluminum; matters in long parts and metal assemblies.
Typical ranges, not design allowables

Typical values for unfilled grades at 23 °C; they differ strongly between homopolymer, copolymers and talc- or glass-filled grades. Design with the datasheet of the specific grade and test parts at their service temperature and load.

Injection molding PP

PP fills thin walls easily and cycles fast, but it shrinks and warps more than amorphous plastics such as ABS or PC. Uretyco's injection-molding rules, with PP-specific notes:

  • Wall thickness: Uretyco's DFM guide recommends 1.0–2.5 mm for PP, with 0.6–3.0 mm as the practical range. Keep walls within about 25% of each other to avoid sink and warp; with PP's high shrinkage this matters more than with ABS.
  • Draft: at least 1° per side on outside walls and 0.5–1° on inside walls; textured faces need about 1° more per 0.025 mm of texture depth.
  • Ribs and bosses: rib base at most 60% of the wall, and in PP toward the lower end to limit sink; boss outer diameter about 2× the screw diameter.
  • Living hinges: typically 0.2–0.5 mm thick, with the melt flowing across the hinge line rather than along it. Flexing the hinge right after molding improves its life.
  • Snap fits and undercuts: PP's flexibility lets shallow undercuts be stripped from the mold without side actions, which simplifies closures and clips.
  • Gates: place the gate at the thickest section; hot runners are worth considering above about 5,000 cycles.

3D printing PP (FDM)

PP is also offered for FDM, mainly to test hinges, snap fits and chemical resistance before tooling. It is one of the harder plastics to print: it warps strongly, adheres poorly to most build plates and gives lower, more direction-dependent strength than molded PP. Large or flat printed parts vary more, and printed hinges need testing because orientation strongly affects their life. Uretyco's 3D-printing guidance also warns against expecting printed parts to match injection-molded properties exactly.

Powder bed PP (SLS and MJF)

PP is also processed as a powder by powder bed fusion: on SLS, and on MJF where a PP powder is available. Parts need no supports and are far less direction-dependent than FDM PP, so powder-bed PP suits functional prototypes and low-volume parts that need PP chemistry and behavior without tooling. Strength and especially elongation at break stay below molded PP. The material is less widespread than PA12 and PA11, so availability, process and lead time are confirmed in the quote and the order. Practical points:

  • Living hinges: printed PP hinges flex better than printed PA12 hinges, but they need thicker sections than molded hinges and reach a much lower cycle life. Test the hinge geometry on a printed sample.
  • Chemical resistance: printed PP keeps the base polymer's resistance to most acids, alkalis and aqueous chemicals and absorbs almost no water, which suits fluid-handling parts, containers and laboratory fittings.
  • Low density: at about 0.9 g/cm³ it is lighter than PA12 (about 1.0 g/cm³), which matters for large housings and ducts.
  • Weldability: printed PP can be thermally welded to other PP parts, including molded ones, for example by hot-plate or hot-gas welding. Adhesives remain unreliable, as on molded PP.
  • Dimensions: PP tends to shrink and warp more than PA12 in the powder bed, and large flat areas and long thin walls are most at risk. Expect wider tolerances than for PA12, stiffen flat panels with ribs or curvature, and validate fit-critical features on a print; final values are confirmed in the quote and the order.

Tolerances and surface

Uretyco's default tolerances for molded parts follow DIN ISO 20457 (formerly DIN 16742); anything tighter belongs on the drawing. Because PP shrinks more, and more variably, than amorphous resins, the same part holds wider tolerances in PP than in ABS or PC, and critical fits should be reviewed against mold-shrink data. Surface finishes range from SPI A1 (mirror) to D3 (rough blast); PP takes textures well, which also hides flow lines and sink. For printed PP, accuracy depends on orientation and part size, so validate fit-critical features on a prototype.

Decoration and joining

PP is normally used as molded, with color from masterbatch and texture built into the tool. Its low surface energy makes printing, painting and gluing harder than on ABS.

OptionWhat it addsNotes for PP
Molded textureGrip, hides flow lines and sinkNeeds extra draft; specify the texture standard and depth.
Through-color (masterbatch)Color without coatingMatch to RAL or a sample; natural PP is translucent white.
Pad printing or paintingLogos and graphicsRequires surface activation (flame, plasma or corona) or an adhesion promoter.
Laser markingCodes and logosNeeds a laser-markable grade or additive.
Welding and mechanical joiningAssemblyHot-plate or vibration welding, snap fits and screws work better than adhesives.
Design out the glue

Adhesives and paint are unreliable on untreated PP. Use snap fits, living hinges, screws into bosses or thermal welding instead, and specify surface activation on the drawing if printing or painting cannot be avoided.

Cost and lead-time drivers

For molded PP the resin is cheap; tooling and cycle time dominate.

  • Tooling: for runs under about 10,000 parts, Uretyco's DFM guide puts aluminum tooling at typically 50–65% cheaper than steel, delivered in 2–3 weeks; above about 25,000 parts hardened steel pays for itself. Bridge tooling lets you start in aluminum and move to steel later.
  • Part design: undercuts that need slides, uneven walls, tight tolerances and cosmetic gate requirements add tool cost and risk, and changes after the tool is cut are expensive.
  • Quantity: setup and tooling spread over volume, so quote realistic quantities for each stage.
  • Printed prototypes: FDM PP has no tooling cost but costs more per part and does not represent molded properties.
  • Documents: material certificates, inspection reports and first-article approval are opt-in and should be requested at quote time.

PP vs. common alternatives

MaterialStiffnessHeat resistance under loadChemical resistanceCold impactRelative cost
PP (homopolymer)BaselineBaselineExcellentPoor; copolymers goodBaseline (lowest)
HDPELowerLowerExcellentVery goodSimilar
ABSHigherHigherFair; attacked by many solventsGoodHigher
POM (acetal)Much higherHigherVery good, except strong acidsModerateHigher
PA12HigherHigherVery good with oils and fuelsGoodHigher

Where you need PP chemistry with better low-temperature impact, specify an impact copolymer. Where you need more stiffness, talc- or glass-filled PP closes part of the gap to ABS at lower cost, with lower shrinkage but a higher density. POM is the step up for precise, low-friction moving parts.

When not to choose PP

Common mismatches

Tight tolerances and precision fits: shrinkage is high and variable. Continuous loads, especially when warm: PP creeps. Service above about 100 °C. Cold-impact parts in homopolymer. Outdoor use without UV stabilization: unstabilized PP chalks and embrittles. Printed, painted or glued surfaces without surface treatment. Contact with aromatic or chlorinated solvents or strong oxidizers. Flame-retardancy requirements beyond UL 94 HB without a flame-retardant grade.

Typical applications

  • Flip-top caps, closures and boxes with living hinges.
  • Containers, laboratory and medical disposables.
  • Automotive interior trim, battery cases and fan shrouds.
  • Appliance housings and internal parts.
  • Chemical tanks, pump parts and fittings.
  • Storage boxes, crates and packaging.

Specifying PP on Uretyco

  1. 1
    Select PP and the grade family

    State homopolymer, random or impact copolymer, filler, color (RAL or sample), UV stabilization and any food-contact requirement.

  2. 2
    Upload STEP plus a drawing

    Show parting-line direction, gate preference, texture, critical dimensions and hinge or snap-fit features.

  3. 3
    Plan prototypes before tooling

    Validate hinges and snaps with printed or bridge-tool parts before freezing a steel tool; request first-article approval in the order scope.

FAQ

Homopolymer or copolymer?

Homopolymer is stiffer and more heat-resistant but brittle near freezing. Impact copolymer is tougher, especially in the cold, at slightly lower stiffness. Random copolymer is clearer and more flexible. If the part may be dropped or used outdoors in winter, choose an impact copolymer.

Is PP food-safe?

Many PP grades are formulated for food contact (for example under FDA 21 CFR 177.1520 or EU Regulation 10/2011), but compliance belongs to the specific grade, colorant and use conditions. State the requirement in the order and request the declaration of compliance at quote time.

Can PP be used outdoors?

Only with UV stabilization; black grades with carbon black last longest. Unstabilized PP chalks, fades and becomes brittle in sunlight. Name the outdoor requirement so the grade and color can be selected accordingly.

Why do PP parts warp?

As a semi-crystalline plastic, PP shrinks more in the flow direction than across it and more in thick areas than in thin ones. Uniform walls, ribs instead of thick sections, good gate placement and textured rather than glossy faces keep warpage and visible sink under control.

Related materials

Was this page helpful?

Can't find what you need? Contact our team for expert assistance with your manufacturing project.

Contact our team