ASA (acrylonitrile styrene acrylate) is an amorphous thermoplastic closely related to ABS. Both have a rigid styrene-acrylonitrile matrix toughened by rubber particles, but ASA uses a saturated acrylate rubber instead of the butadiene in ABS. That one change gives ASA its defining property: it keeps its color, gloss and impact strength in sunlight, where ABS yellows and becomes brittle.
Choose ASA for parts that live outdoors or behind glass: enclosures, housings, automotive exterior trim, signage and garden equipment. On Uretyco it is available as an FDM filament for prototypes and low volumes, and as an injection-molding resin once the design is stable and quantities justify tooling.
Mechanical and physical properties
| Property | Typical value | Notes |
|---|---|---|
| Tensile strength | ≈ 40–50 MPa | Molded; FDM parts are somewhat lower in the layer plane and much lower across layers. |
| Elongation at break | ≈ 10–40% | Strongly grade-dependent; far lower in FDM parts, especially across layers. |
| Tensile modulus | ≈ 2.0–2.5 GPa | Similar to ABS. |
| Density | ≈ 1.07 g/cm³ | Similar to ABS. |
| Heat deflection temperature | ≈ 85–100 °C | At 0.45 MPa; grade-dependent. |
| Max service temperature | ≈ 70–85 °C | Dark colors in direct sun run hotter than the surrounding air. |
| UV and weathering | Excellent | Keeps color and impact strength outdoors far better than ABS; pigment choice affects fading. |
| Chemical resistance | Moderate | Resists water, dilute acids and many oils; attacked by ketones such as acetone, esters and aromatic solvents. |
| Molding shrinkage | ≈ 0.4–0.7% | Typical of amorphous styrenics. |
Typical values for unfilled general-purpose grades. Molded and printed parts differ, and FDM properties depend on orientation, layer height and infill. Check the datasheet of the exact grade and validate load-bearing parts with real samples.
Processing routes
FDM printing
ASA prints like ABS: it needs a heated bed and ideally an enclosed build chamber, because large flat parts warp and layers can separate when they cool unevenly. Design and ordering points:
- Orientation: layer adhesion is the weak direction; orient clips, bosses and loaded features along the layers.
- Large flat areas: add ribs or split large panels, since long flat parts are most prone to warping and corner lift.
- Fits and threads: allow clearance, drill fit-critical holes and use heat-set inserts for threads; Uretyco's 3D printing guidance recommends testing fit-critical features before production.
- Surface: like ABS, ASA can be acetone-vapor smoothed for a sealed, glossy finish, at some loss of sharp detail.
Injection molding
In molding, ASA behaves much like ABS, so the ABS guidance in Uretyco's injection molding DFM article is a sound starting point: about 2.0–2.5 mm nominal wall (1.0–4.0 mm range), uniform thickness, and at least 1° of draft on outside walls, more for textures. For runs under about 10,000 parts, aluminum tooling is typically 50–65% cheaper than steel and ships in 2–3 weeks; steel tooling pays off at higher volumes. Molded-in color avoids painting and keeps scratches less visible.
Tolerances and surface
Without a drawing tolerance, FDM parts on Uretyco follow the default of ±0.5 mm or ±0.5%, whichever is greater; actual results vary with orientation, part size, supports and post-processing, so test fit-critical features first. Molded tolerances depend on shrinkage and geometry; critical fits are reviewed against mold shrink data and may need secondary machining. Molded surfaces follow SPI finishes from A1 (mirror) to D3 (rough blast); call out anything else on the drawing.
Finishing options
| Finish | Process | Notes for ASA |
|---|---|---|
| As-printed or as-molded | FDM, molding | Molded-in color needs no further finish; FDM parts show layer lines. |
| Acetone vapor smoothing | FDM | Sealed, glossy surface; softens sharp edges and fine detail. |
| Sanding, priming and painting | FDM, molding | Paints well; specify a RAL code or sample. |
| Molded texture | Molding | Hides sink marks and scratches; needs extra draft, about 1° per 0.025 mm of texture depth. |
UV resistance comes from the polymer, but color fastness depends on the pigment. For long outdoor life, prefer colors the material supplier rates for weathering, and remember that dark parts in direct sun run much hotter than the air.
Cost and lead-time drivers
The cost structure depends on the process:
- FDM: priced on volume, build time, supports and post-processing. ASA costs a little more than PLA or PETG and needs enclosed printers.
- Injection molding: tooling dominates at low volumes; unit cost falls with quantity, cycle time and cavity count.
- Design changes: changes after the tool is cut are expensive, so validate fit and function with FDM parts first.
- Color and texture: custom colors and textured tools add lead time.
ASA vs. common alternatives
| Material | Outdoor / UV | Heat resistance | Impact | Processes | Notes |
|---|---|---|---|---|---|
| ASA | Excellent | ≈ 70–85 °C | Good | FDM, injection molding | The outdoor default among styrenics. |
| ABS | Poor; yellows and embrittles | ≈ 60–80 °C | Good | CNC, injection molding, FDM | Slightly cheaper for indoor parts. |
| PETG | Moderate | ≈ 60–70 °C | Good | FDM, CNC, injection molding | Easier to print; less weather-resistant. |
| PC | Moderate; needs UV-stabilized grades | ≈ 115–125 °C | Excellent | CNC, injection molding | For heat and impact; can be transparent. |
| PLA | Poor | ≈ 50 °C | Low | FDM | Indoor prototypes only. |
If a part must survive years of sun and weather, ASA is usually the most economical styrenic choice. Move to PC when heat or impact demands it, and to polyamide or polypropylene families when chemical resistance matters more than appearance.
When not to choose ASA
Continuous temperatures above about 85 °C: consider PC or a polyamide. Contact with solvents such as acetone, fuels or aromatics. Transparent parts: ASA is opaque, so use PC or PMMA. Highly loaded, creep-critical structures. Flame-retardancy requirements: confirm that a rated grade exists before designing around ASA.
Typical applications
- Outdoor electrical and telecom enclosures, antenna housings.
- Automotive exterior trim, mirror housings and grilles.
- Signage letters and architectural components.
- Garden, pool and outdoor-equipment parts.
- Camera, sensor and drone housings for outdoor use.
Specifying ASA on Uretyco
- 1Choose the process
FDM for prototypes and low volumes; injection molding when the design is frozen and the quantity justifies tooling.
- 2Upload the right files
STL, 3MF or STEP for printing; STEP plus a drawing with draft, parting line, gate preference and texture for molding.
- 3Specify color and environment
Give a RAL code or sample, the visible faces and the outdoor exposure so the right grade and finish are chosen.
FAQ
ASA or ABS?
Indoors, ABS is slightly cheaper and performs similarly. Anywhere with sunlight or weather, choose ASA: ABS yellows and loses impact strength within months outdoors, while ASA keeps both.
Can FDM ASA parts be smoothed?
Yes. Like ABS, ASA responds to acetone vapor smoothing, which seals the surface and hides layer lines but rounds fine edges. Sanding and painting are the alternatives.
Are printed ASA parts as UV-stable as molded ones?
The polymer is the same, so UV resistance is similar. Printed parts have layer seams and lower mechanical properties, however, so validate outdoor printed parts for the load they carry.
When should I move from FDM to molding?
When the design is stable and the quantity justifies tooling. Uretyco can compare both routes; aluminum tooling suits runs under about 10,000 parts, steel tooling higher volumes.
Related resources
- ABSThe indoor counterpart.
- PETGEasy-printing, tough FDM material.
- Polycarbonate (PC)Higher heat and impact resistance.
- PLAFor indoor visual prototypes.
- 3D PrintingTechnologies, files and cost drivers.
- Injection MoldingTooling economics and design rules.
- Injection Molding DFMWalls, draft, gates and tooling choice.
- Engineering Plastics ComparedABS, PC, PEEK and PA12 side by side.
Related materials
Can't find what you need? Contact our team for expert assistance with your manufacturing project.