Uretyco
Make it now
Polycarbonate (PC)

Polycarbonate (PC)

Plastics
PCPolycarbonatePlasticImpact

Polycarbonate (PC) reference: typical properties, CNC machining and injection molding rules, clarity and polishing, chemical limits, cost drivers, and comparison with PMMA, ABS, PETG and PEEK.

Polycarbonate (PC) is an amorphous, transparent thermoplastic that combines high impact strength with good stiffness, heat resistance up to about 115–125 °C and light transmission close to that of glass at under half its density. It machines and molds well and holds dimensions better than most unfilled plastics.

Choose PC for machine guards, safety covers, sight windows and housings that will be knocked, dropped or struck. Its weak points are chemical stress cracking (solvents, some cleaners and oils), a soft surface that scratches easily, and yellowing under UV unless the grade is stabilized or coated. On Uretyco it is offered for CNC machining and injection molding; FDM printing in PC can also be requested.

Mechanical and physical properties

PropertyTypical valueNotes
Tensile strength (yield)≈ 60–65 MPaYields in a ductile way and elongates far beyond yield.
Elongation at break≈ 100–150%Notches, thick sections and solvent attack sharply reduce ductility.
Tensile modulus≈ 2.3–2.4 GPaSimilar to ABS; stiffness has to come from geometry.
Notched impact strength (Izod)≈ 600–900 J/mASTM D256, 3.2 mm specimens. Several times general-purpose ABS; lower in thick sections and at sharp notches.
Density1.20 g/cm³Under half the density of glass.
Heat deflection temperature (HDT)≈ 125–140 °CAt 1.8 MPa.
Glass transition≈ 145–150 °CUpper limit for short exposures.
Max. continuous service temperature≈ 115–125 °CNot for continuous hot water or steam: PC hydrolyses above about 60 °C.
Light transmission≈ 88–90%Clear grades, ≈ 3 mm. Machined faces stay translucent until polished.
Thermal expansion≈ 65–70 µm/m·KNearly 3× aluminum.
FlammabilityUL 94 HB to V-0Grade- and thickness-dependent; flame-retardant grades reach V-0.
Typical values, not design allowables

Typical room-temperature values for general-purpose, unfilled PC as extruded sheet and rod or standard molding grades. Glass-filled, flame-retardant, UV-stabilized and optical grades differ. For design calculations, use the data sheet of the specific grade named in your quote.

CNC machining PC

PC machines cleanly and, unlike PMMA, does not chip at edges. It is, however, notch- and chemical-sensitive, so the process must avoid heat build-up, surface stress and the wrong fluids. Watch for:

  • Coolants and cleaners: use air or plain water-based coolant. Many oils, solvents and some alcohol-based cleaners cause stress cracking, sometimes days after machining.
  • Residual stress: heavy cuts and dull tools stress the surface; for clear or chemically exposed parts, annealing after rough machining lowers the cracking risk.
  • Walls and corners: the CNC Design Guide's values for POM, 1.5 mm minimum wall and 3:1 pocket depth-to-width, are a sensible floor. Keep internal radii at least one-third of the pocket depth and avoid sharp notches, PC's main failure trigger.
  • Threads and fasteners: tapped M2–M10 threads, 1.5–3× the diameter deep, or heat-set inserts for repeated assembly. Avoid tapered threads and over-tightened screws, which stress-crack PC.

Injection molding PC

PC molds into tough, glossy and optically clear parts, but its high melt viscosity and notch sensitivity make wall design and gating important. From Uretyco's injection molding DFM guide:

  • Wall thickness: 2.0–3.0 mm recommended, 1.0–4.0 mm as practical limits; keep wall variation under about 25%.
  • Draft: at least 1° per side outside and 0.5° or more inside; add about 1° per 0.025 mm of texture depth.
  • Ribs, bosses and radii: rib base no more than 60% of the wall and screw bosses about 2× the screw diameter outside. Generous radii at rib roots and corners matter more for PC than for most resins.
  • Gates: at the thickest section, with weld lines kept away from load paths and windows. For optical parts, specify SPI A-grade polish on the faces that must be clear.
  • Drying: PC must be dried thoroughly before molding; wet resin degrades and gives splay marks and brittle parts.

Tolerances and surface finish

For machined PC, Uretyco treats unspecified tolerances as ISO 2768-mK, with a default surface of about Ra 1.6–3.2 µm and light deburring; tighter tolerances need a 2D drawing and belong on functional features only. Molded parts follow DIN ISO 20457 (formerly DIN 16742) by default, with SPI finishes from A1 (mirror) to D3 (rough blast). PC expands nearly three times as much as aluminum, so inspect tight fits on large parts at 20 °C. Final values are confirmed in the quote and the order.

FDM printing of PC

PC is also printed as filament by FDM when a printed part needs more heat resistance and toughness than ABS or PETG offer. It is one of the more demanding filaments, and printed PC is translucent at best, so parts that must be clear are still machined and polished, or molded. Points to consider:

  • Temperatures and enclosure: PC prints at a nozzle temperature of about 260–300 °C on a bed at about 100–120 °C, ideally in a heated, enclosed chamber. Without one, large parts warp, lift at the corners and crack between layers; ribs and rounded corners help, while large solid sections make warping worse. FDM tolerances depend on orientation, part size and supports, so test fit-critical features first.
  • Moisture: PC filament absorbs moisture, and wet material degrades when it is melted, causing bubbles, rough surfaces and brittle parts. It must be dried before printing and kept dry during the build.
  • PC blends: PC-ABS prints more easily and warps less, with lower heat resistance than pure PC; flame-retardant and fiber-filled PC grades also exist. The exact grade is confirmed in the quote.
  • Compared with ABS and PETG: printed PC is stronger and tougher and keeps its shape at higher temperatures. The base polymers reach heat deflection temperatures of about 125–140 °C for PC, 80–100 °C for ABS and 65–70 °C for PETG. As with all FDM parts, strength across the layers (Z) is markedly lower, so printed PC does not reach the impact strength of machined or molded PC.

Finishing and clarity

Machined PC faces are translucent, so clarity has to be restored. Decide early which faces must be optically clear and mark them on the drawing.

FinishWhat it addsNotes for PC
As-machinedLowest costMatte, translucent faces with tool marks; fine for opaque or functional parts.
Bead blastEven, frosted lookDiffuses light evenly; typically +5–10% on CNC quotes.
Mechanical polishClear, glossy facesRestores transparency on flat and simple faces; mirror polish (Ra < 0.4 µm) typically +50–150% on CNC quotes.
Vapor polishClear complex facesReaches pockets and curved faces; uses solvent vapor, so stress-relieve first or the part may craze.
Hard-coated stockScratch and UV resistanceSupplied as coated sheet; machined edges and faces remain uncoated.

Cost and lead-time drivers

PC stock costs roughly 1.5× ABS, but on machined parts the price is driven more by machining and polishing. As a rule of thumb, material is typically 10–30% of a CNC quote and machine time 35–55%. The main levers:

  • Clarity: every polished face adds manual work; specify optical faces only where they are needed.
  • Tooling: for runs under about 10,000 parts, aluminum tooling is typically 50–65% cheaper than steel and ships in 2–3 weeks; hardened steel pays off from about 25,000 parts.
  • Grade: clear general-purpose sheet and rod are common; UV-stabilized, flame-retardant, coated or colored grades can add lead time.
  • Documents: material certificates and inspection reports are opt-in and can extend the lead time. Request them at quote time.

PC vs. common alternatives

MaterialImpactClarityService temperatureSurface / UVRelative cost
PCVery high≈ 88–90%≈ 115–125 °CSoft surface; yellows without UV gradeBaseline
PMMALow; brittle≈ 92%≈ 70–90 °CHarder surface; excellent UV resistanceLower
ABSGoodOpaque≈ 60–80 °CPoor UV resistanceLower (PC ≈ 1.5× ABS)
PETGGood≈ 85–90% (sheet)≈ 60–70 °CFairLower
PEEKGoodOpaque≈ 250 °CExcellent chemical resistanceMuch higher

Choose PMMA when clarity, scratch resistance and outdoor weathering matter and nothing will hit the part; choose PC when it might be hit. PETG is a lower-cost clear option for indoor covers that do not need PC's heat resistance.

When not to choose PC

Common mismatches

Contact with solvents, fuels, ammonia- or amine-based cleaners, or many oils while under stress: consider POM, PA12 or PEEK. Continuous hot water or steam: PC hydrolyses, so consider PEEK. Outdoor glazing without a UV-stabilized or hard-coated grade. Clear faces exposed to abrasion: use PMMA or coated PC. Highly loaded parts with sharp notches or tight press fits.

Typical applications

  • Machine guards, safety covers and inspection windows.
  • Clear or tinted housings, lenses and light covers.
  • Electrical enclosures and insulating parts.
  • Lab and medical device housings (check sterilization compatibility).
  • Protective visors and face shields.
  • Prototype housings that must survive drop tests.

Specifying PC on Uretyco

  1. 1
    Select PC and the process

    CNC for prototypes and small batches, injection molding for stable designs in volume.

  2. 2
    Name the grade

    Clear or colored, UV-stabilized, flame-retardant or hard-coated: state it in the order notes so availability is confirmed in the quote.

  3. 3
    Mark optical and cosmetic faces

    Show on the 2D drawing which faces must be clear or polished, plus tolerances tighter than ISO 2768-mK and threads.

  4. 4
    Request documents at quote time

    Material certificates and inspection reports are opt-in.

FAQ

How much tougher is PC than ABS or acrylic?

In notched Izod tests, general-purpose PC typically reaches several times the value of standard ABS and tens of times that of PMMA. The advantage shrinks at sharp notches, in thick sections and after solvent attack, so design generous radii and validate critical guards under realistic impact.

Can a machined PC part be fully transparent?

Yes, but only after polishing. Flat faces can be machine- or hand-polished; complex faces are usually vapor-polished. Faces left from the original extruded sheet stay clear, so orient the part so that they fall where clarity matters most.

Is PC suitable for outdoor use?

With the right grade. Standard PC yellows and loses toughness under prolonged UV; UV-stabilized or hard-coated sheet is used for outdoor glazing and covers. State outdoor exposure in the order notes.

Related materials

Was this page helpful?

Can't find what you need? Contact our team for expert assistance with your manufacturing project.

Contact our team