POM (polyoxymethylene, acetal) is a semi-crystalline engineering plastic with high stiffness, low friction, excellent wear and fatigue behavior and very low moisture uptake. Delrin is the best-known homopolymer (POM-H); copolymer grades (POM-C) are sold under names such as Hostaform, Celcon and Acetron. It is one of the easiest plastics to machine to tight tolerances.
Choose POM for gears, bushings, rollers, cams, snap-fits, valve parts and any precise plastic part that slides or moves. Its limits: it burns readily, is attacked by strong acids, oxidizers and chlorine, has limited UV resistance, and is very hard to bond. On Uretyco it is offered for CNC machining and injection molding.
Mechanical and physical properties
| Property | Typical value | Notes |
|---|---|---|
| Tensile strength (yield) | ≈ 70 MPa (POM-H); ≈ 60–65 MPa (POM-C) | The homopolymer is stronger and stiffer. |
| Elongation at break | ≈ 20–40% | Grade-dependent. |
| Tensile modulus | ≈ 2.8–3.2 GPa | Among the stiffest unfilled engineering plastics. |
| Density | ≈ 1.41–1.42 g/cm³ | Heavier than most plastics. |
| Melting point | ≈ 175 °C (POM-H); ≈ 165 °C (POM-C) | Sharp melting point; no gradual softening. |
| Max. continuous service temperature | ≈ 90–105 °C | Short peaks up to ≈ 140 °C. |
| Coefficient of friction (dry, vs. steel) | ≈ 0.2–0.35 | Self-lubricating; PTFE-filled grades go lower. |
| Thermal expansion | ≈ 100–120 µm/m·K | About 5× aluminum: a 100 mm part grows ≈ 0.1–0.12 mm per 10 °C. |
| Water absorption | ≈ 0.2% (24 h); ≈ 0.8% saturated | Far lower than nylon, so fits stay stable in humid conditions. |
| Flammability | UL 94 HB | Burns with an almost invisible flame and releases formaldehyde. |
| Machinability | Excellent | Free-cutting, forms clean chips and holds tight tolerances. |
Typical room-temperature values for unfilled extruded POM-H and POM-C stock and standard molding grades. Glass-filled, PTFE-filled, ESD and food-contact grades differ. For design calculations, use the data sheet of the specific grade named in your quote.
CNC machining POM
POM is one of the best plastics to machine: it cuts much like free-machining brass, forms clean chips and holds tight tolerances. Uretyco's CNC Design Guide lists it with a 1.5 mm minimum wall and a 3:1 maximum pocket depth-to-width ratio. Watch for:
- Walls and pockets: thinner walls or deeper pockets flex under cutting forces and spring back after machining.
- Centerline porosity: thick POM-H (Delrin) rod and plate can be porous at the center. For pressure-tight or highly stressed parts from thick stock, specify POM-C or porosity-free stock.
- Stress and warp: large, asymmetric parts can move after roughing; leave stock for a finishing pass on critical faces.
- Internal corners: keep radii at least one-third of the pocket depth; POM cannot be EDM-machined.
- Threads: tapped M2–M10 threads, 1.5–3× the diameter deep, hold well; use heat-set or threaded inserts where screws are often reassembled.
Injection molding POM
POM flows easily and fills thin walls, but as a semi-crystalline resin it shrinks much more than ABS or PC (≈ 1.8–2.2%) and differently along and across the flow. Uretyco's injection molding guide names POM as the usual choice for wear surfaces; apply the DFM rules with extra attention to uniformity:
- Wall thickness: stay in the general 1.5–3.5 mm sweet spot and keep variation under about 25%; thick sections sink and form voids.
- Draft: at least 1° per side outside and 0.5° or more inside; add about 1° per 0.025 mm of texture depth.
- Ribs, bosses and snap-fits: rib base no more than 60% of the wall and bosses about 2× the screw diameter outside. POM's springiness suits snap-fits.
- Gears and precision parts: gate so that flow is symmetrical around bores and teeth; critical fits need a tolerance-stack review against shrink data.
- Processing: overheated POM degrades and releases formaldehyde, so melt temperature and residence time must be controlled.
Tolerances and surface finish
Uretyco treats unspecified CNC tolerances as ISO 2768-mK, with a default surface of about Ra 1.6–3.2 µm and light deburring. POM can hold considerably tighter tolerances on functional features, which then need a 2D drawing. Because POM expands about five times as much as aluminum, state the measuring temperature for tight bores and gear data and allow running clearance at operating temperature. Molded parts follow DIN ISO 20457 (formerly DIN 16742) by default. Final values are confirmed in the quote and the order.
Design notes for gears, bushings and sliding parts
- Pairing: POM running against steel or against nylon wears little; POM against POM wears faster under load.
- Clearance: plastic bushings need more running clearance than bronze, because heat and expansion close the gap; check the gap at the highest operating temperature.
- Heat: frictional heat limits load and speed; thin bushing walls and a metal housing help dissipate it.
- Lubrication: POM runs dry, but an initial grease film extends the life of gears and heavily loaded sliding parts.
Finishing options
POM is normally used as-machined or as-molded; it accepts paint and adhesives poorly. Options:
| Finish | What it adds | Notes for POM |
|---|---|---|
| As-machined | Lowest cost | Smooth, slightly glossy faces; natural white or black. |
| Bead blast | Uniform matte look | Typically +5–10% on CNC quotes; avoid on sliding faces. |
| Fine-machined functional faces | Low friction, sealing | Specify Ra only on running and sealing faces. |
Cost and lead-time drivers
POM is a moderately priced engineering plastic that cuts quickly, so machined parts are usually economical. As a rule of thumb, material is typically 10–30% of a CNC quote and machine time 35–55%. The main levers:
- Grade and color: natural and black POM-H and POM-C stock are common; filled, ESD, food-contact or colored grades can add lead time.
- Tolerances: tight tolerances on many features add inspection; reserve them for bores, gear data and fits.
- Tooling: for runs under about 10,000 parts, aluminum tooling is typically 50–65% cheaper than steel and ships in 2–3 weeks; hardened steel pays off from about 25,000 parts.
- Documents: material certificates and inspection reports are opt-in and can extend the lead time. Request them at quote time.
POM vs. common alternatives
| Material | Stiffness | Friction and wear | Moisture uptake | Max. service | Relative cost |
|---|---|---|---|---|---|
| POM-H (Delrin) | ≈ 3.0–3.2 GPa | Very good | Very low | ≈ 90–105 °C | Baseline |
| POM-C | ≈ 2.8 GPa | Very good | Very low | ≈ 100 °C | Similar |
| PA6 / PA66 (nylon) | ≈ 1.5–3 GPa, moisture-dependent | Very good; tougher under impact | High; dimensions change | ≈ 80–100 °C | Similar |
| UHMW-PE | ≈ 0.7–0.8 GPa | Excellent abrasion resistance, very low friction | Negligible | ≈ 80 °C | Lower |
| PEEK | ≈ 3.6–4.2 GPa | Excellent, also at high temperature | Very low | ≈ 250 °C | Much higher |
Pick POM-C over POM-H for hot water, alkaline cleaning or thick parts where centerline porosity matters; pick POM-H for maximum stiffness, strength and fatigue life. Nylon is tougher but swells with moisture; PEEK takes over above about 100 °C or in aggressive chemicals.
When not to choose POM
Strong acids, oxidizers or chlorinated water, including pool and many disinfectant chemicals: consider PP, PVDF or PEEK. Continuous service above about 100 °C: consider PEEK. Glued assemblies: design for screws, snap-fits or press fits instead. Fire-sensitive applications: POM burns readily with an almost invisible flame. Long outdoor exposure without a UV-stabilized black grade.
Typical applications
- Precision gears, sprockets and worm wheels.
- Bushings, bearings, rollers and wear strips.
- Snap-fit housings, clips and fasteners.
- Valve and pump parts for fluid handling (not in chlorinated water).
- Jigs, fixtures and nests for assembly and testing.
- Food-processing machine parts (food-contact grades).
Specifying POM on Uretyco
- 1Select POM and the process
CNC for prototypes, precision parts and small batches; injection molding for stable designs in volume.
- 2Choose homopolymer or copolymer
POM-H (Delrin) for maximum stiffness and fatigue strength, POM-C for hot water, alkaline cleaning and thick stock; note color and any food-contact or ESD requirement in the order notes.
- 3Upload STEP plus a 2D drawing
Show bores, fits and gear data with tolerances, and the measuring temperature for tight features.
- 4Request documents at quote time
Material certificates and inspection reports are opt-in.
FAQ
Is Delrin the same as POM or acetal?
Delrin is a brand of acetal homopolymer (POM-H). Acetal or POM also covers copolymer grades (POM-C), which are slightly less stiff but more resistant to hot water and alkalis and free of centerline porosity in thick stock. If either is acceptable, say so in the order notes to widen supply.
Can POM be glued?
Only poorly. Most adhesives do not wet POM, and surface treatments are rarely reliable for load-bearing joints. Use screws into tapped holes or inserts, snap-fits, press fits or ultrasonic welding instead.
How tight can POM parts be machined?
POM is one of the most precise plastics to machine, but it expands about five times as much as aluminum. Tolerances finer than the default ISO 2768-mK belong on a drawing, together with the measuring temperature for critical features; achievable values are confirmed in the quote.
Can POM be 3D printed?
Only with difficulty. POM filament exists, but it adheres poorly to standard print beds, for the same reason it is hard to glue, and it shrinks strongly as it crystallizes, so parts warp, lift at the corners and lose accuracy. Overheated POM also releases formaldehyde, so printing needs an enclosed, well-ventilated machine. Because POM machines quickly to tight tolerances and molds well, machined or molded parts are almost always the better route for gears, bushings and sliding parts; on printed parts, layer lines also raise friction and wear. A printed POM part is acceptable for a small, lightly loaded prototype that checks fit or motion where accuracy is not critical; for printed sliding parts, PA12 by MJF or SLS is the usual alternative. Feasibility of printed POM is confirmed in the quote.
Related resources
- PEEKFor temperatures above about 100 °C and aggressive media.
- Polycarbonate (PC)Tough and transparent, but not a bearing material.
- ABSLower-cost housings and covers.
- CNC Design GuideTolerances, walls, threads and setups.
- CNC MachiningProcess overview, files and cost drivers.
- Injection Molding DFMWalls, draft, ribs, gates and tooling.
- Injection MoldingWhen molding pays off and what to upload.
- Technical Drawings & TolerancesWhat belongs on the 2D drawing.
Related materials