Uretyco
Make it now
PMMA (Acrylic / Plexiglas)

PMMA (Acrylic / Plexiglas)

Plastics
PMMAAcrylicPlexiglasClear

PMMA (acrylic) reference: cast vs extruded sheet, typical properties, CNC machining and laser-cutting guidance, edge finishing, stress cracking, cost drivers, and comparison with PC, PETG and glass.

PMMA (polymethyl methacrylate, acrylic; trade names include Plexiglas and Perspex) is an amorphous, glass-clear thermoplastic. It transmits about 92% of visible light, weathers outdoors for years without yellowing, has a harder, more scratch-resistant surface than other clear plastics, and polishes to optical quality. It is, however, brittle: it cracks rather than bends.

Choose PMMA for displays, light guides, lenses, covers, signage, windows and sight glasses where clarity and appearance matter and impact loads are low. It comes as cast sheet (better optics, machinability and chemical resistance) or extruded sheet (cheaper, more uniform thickness, more sensitive to solvents and stress). On Uretyco it is offered for CNC machining and laser cutting.

Mechanical and physical properties

PropertyTypical valueNotes
Tensile strength≈ 60–75 MPaCast sheet at the upper end.
Elongation at break≈ 2–5%Brittle; fails without yielding.
Tensile modulus≈ 3.0–3.3 GPaStiffer than PC or PETG.
Notched impact strength (Izod)≈ 15–25 J/mASTM D256. A small fraction of PC, yet many times more impact-resistant than glass of the same thickness.
Density≈ 1.18–1.19 g/cm³Less than half the density of glass.
Light transmission≈ 92%Clear, 3 mm; refractive index ≈ 1.49.
Surface hardnessRockwell M ≈ 90–100Harder than PC or PETG, but scratches more easily than glass.
Max. continuous service temperature≈ 70–90 °CExtruded sheet at the lower end.
Thermal expansion≈ 70–80 µm/m·KAbout 3× aluminum and 8× glass; allow for it in frames and fixings.
FlammabilityUL 94 HBBurns steadily; not for fire-rated glazing without a certified grade.
Typical values, not design allowables

Typical room-temperature values for general-purpose cast and extruded PMMA sheet. Impact-modified, UV-transmitting, colored and mirrored grades differ. For design calculations, use the data sheet of the specific grade named in your quote.

CNC machining PMMA

PMMA machines well, cast sheet especially, but it is brittle and notch-sensitive, so the process must avoid chipping, heat and residual stress. Watch for:

  • Chipping: sharp single- or two-flute cutters, moderate feeds and support under the cut prevent edge chipping and breakout at hole exits.
  • Heat and stress: extruded sheet melts and gums more easily, so use air or water cooling. Machined edges carry stresses that can craze later on contact with solvents or alcohol-based cleaners; annealing after machining reduces the risk.
  • Walls and corners: the CNC Design Guide's values for POM (1.5 mm minimum wall, 3:1 pocket depth-to-width) are a sensible floor. Keep internal radii at least one-third of the pocket depth and avoid sharp internal corners in load paths, where PMMA cracks.
  • Holes and fixings: drill with zero-rake drills. Tapped threads in PMMA are weak and crack-prone, so prefer through-bolts with washers in slightly oversized holes that allow for thermal expansion, and never over-tighten.

Laser cutting PMMA

PMMA is one of the best materials for CO₂ laser cutting: the cut edge comes out glossy and flame-polished, without tool marks. Uretyco's laser-cutting guidance covers acrylic sheet, and the usual DXF rules apply:

  • DXF: export the flat profile at 1:1 scale with closed contours and no duplicate lines, text, dimensions or title block; state material, thickness and quantity separately.
  • Small features: avoid holes smaller than the sheet thickness unless reviewed, and keep narrow bridges and slots realistic for the thickness.
  • Corners: add small radii or reliefs at sharp internal corners, which concentrate stress in brittle PMMA.
  • Edge stress: laser-cut edges hold residual stress; keep solvent cements and alcohol cleaners away from them unless the parts are annealed, or they may craze.
  • Edge taper: thick sheet shows a slight taper, so hole diameters differ between top and bottom faces; machine edges that need precise dimensions.

Tolerances and surface finish

For machined PMMA, Uretyco treats unspecified tolerances as ISO 2768-mK, with a default surface of about Ra 1.6–3.2 µm and light deburring; tighter tolerances need a 2D drawing. Laser-cut outlines can be controlled well when the DXF is clean, but the sheet thickness itself varies, especially in cast sheet, so do not tolerance thickness tighter than the sheet supplier delivers. Final values are confirmed in the quote and the order.

Edge and surface finishing

FinishWhat it addsNotes for PMMA
Laser-cut edgeGlossy edge as cutClear, flame-polished look; slight taper on thick sheet.
As-machined edgeLowest cost for machined partsFrosted, translucent edge with tool marks.
Diamond or mechanical polishOptical-quality edges and facesHighest clarity; mirror polish (Ra < 0.4 µm) typically +50–150% on CNC quotes.
Flame polishGlossy edges at low costFast on straight edges; adds edge stress, so avoid before solvent bonding.
Bead blast or sandingFrosted, light-diffusing surfaceTypically +5–10% on CNC quotes; hides fingerprints.
Protective filmScratch protection in transitSheet normally ships with masking film; specify whether it should stay on visible faces.

Cost and lead-time drivers

PMMA sheet is inexpensive; the price is set by the process and the finish. The main levers:

  • Laser cutting: cut length, pierce count and sheet thickness drive machine time; simplify decorative contours and use the thinnest sheet that works.
  • CNC: pockets, 3D surfaces and polished faces add machine and manual time; as a rule of thumb, machine time is typically 35–55% of a CNC quote.
  • Edge finish: polished edges are often the largest single add-on, so specify them only on visible edges.
  • Sheet type and color: clear cast and extruded sheet in standard thicknesses are common; special colors, UV-transmitting or impact-modified grades can add lead time.
  • Documents: material certificates and inspection reports are opt-in and can extend the lead time. Request them at quote time.

PMMA vs. common alternatives

MaterialClarityImpactScratch / UVService temperatureProcesses on Uretyco
PMMA≈ 92%Low; brittleGood scratch resistance; excellent UV≈ 70–90 °CCNC, laser cutting
PC≈ 88–90%Very highSoft surface; needs UV grade≈ 115–125 °CCNC, injection molding
PETG≈ 85–90%GoodSoft; fair UV≈ 60–70 °CFDM, CNC, injection molding
Glass≈ 90–92%Very lowExcellentSeveral hundred °CNot offered

Choose PC when the part may be hit, kicked or dropped, and PMMA when clarity, scratch resistance and weathering matter more. PETG is tougher and easier to bend than PMMA but scratches more easily and is less UV-stable.

When not to choose PMMA

Common mismatches

Machine guards, vandal-prone glazing or anything that may be struck: use PC. Contact with solvents, alcohol, fuels or many cleaners, especially on stressed or laser-cut edges: PMMA crazes. Service above about 80 °C. Thin snap-fits, living hinges or loaded tapped threads. Fire-rated applications without a certified grade.

Typical applications

  • Display cases, stands and point-of-sale fixtures.
  • Signage, lettering and backlit panels.
  • Light guides, diffusers and lenses.
  • Instrument windows, covers and front panels.
  • Architectural and outdoor panels.
  • Models and exhibition pieces.

Specifying PMMA on Uretyco

  1. 1
    Choose laser cutting or CNC

    Laser cutting for flat profiles with polished edges; CNC for pockets, chamfers, 3D shapes, precise hole positions or very thick sheet.

  2. 2
    Specify sheet type and thickness

    Cast or extruded, clear or colored, and nominal thickness; say if either sheet type is acceptable.

  3. 3
    Upload the right files

    A clean 1:1 DXF for laser cutting; STEP plus a 2D drawing for machined parts, tolerances and threads.

  4. 4
    Mark visible edges and faces

    State which edges must be polished and whether the protective film should stay on.

FAQ

Cast or extruded acrylic?

Cast sheet has better optics, machines with less melting, resists solvents better and engraves with a frosted white mark, so it is the safer choice for machined, polished or bonded parts. Extruded sheet is cheaper, more uniform in thickness and laser-cuts cleanly, but it is more prone to stress cracking. For simple laser-cut panels, either works.

How are acrylic parts joined?

Usually with solvent cements, which give clear joints. Solvent bonding attacks stressed edges, so laser-cut or flame-polished edges should be annealed first, or they may craze. Mechanical fixings need oversized holes and washers to allow for thermal expansion.

Is PMMA suitable outdoors?

Yes. PMMA has the best weathering of the common clear plastics and stays clear for years without a coating. Allow for its thermal expansion in frames, and avoid it where hail, vandalism or impact is likely; use PC there.

Related materials

Was this page helpful?

Can't find what you need? Contact our team for expert assistance with your manufacturing project.