TPU (thermoplastic polyurethane) is a thermoplastic elastomer: it stretches and recovers like rubber but melts and processes like a thermoplastic. At Shore 95A it is firm, close to a hard rubber: it bends and absorbs impact but holds its shape. TPU combines very high abrasion and tear resistance with good resistance to oils, greases and many fuels.
Choose TPU 95A for grips, bumpers, protective covers, cable strain reliefs, cushioning lattices, wearable parts and light-duty gaskets. It is not a high-temperature or precision material, and it takes a permanent set under sustained compression more readily than silicone or EPDM. On Uretyco it is offered for MJF and FDM printing and for injection molding.
Mechanical and physical properties
| Property | Typical value | Notes |
|---|---|---|
| Hardness | Shore 95A (≈ 45–50 Shore D) | Firm; softer TPU grades such as 85A or 90A exist. |
| Tensile strength | ≈ 30–50 MPa (molded) | Printed parts reach considerably less; powder-bed TPU often only a fraction. |
| Elongation at break | ≈ 400–600% (molded) | Lower in printed parts, especially across FDM layers. |
| Abrasion resistance | Excellent | Among the best of all elastomers; better than most rubbers. |
| Density | ≈ 1.15–1.22 g/cm³ | Similar to most engineering plastics. |
| Service temperature | ≈ −30 to +80 °C | Short peaks higher; polyether grades stay flexible at lower temperatures. |
| Compression set | Moderate | Higher than silicone or EPDM: sustained squeeze, especially when warm, leaves a permanent set. |
| Hydrolysis resistance | Grade-dependent | Polyether TPU resists hot water and humidity; polyester TPU degrades in hot, wet conditions but resists oils better. |
| Chemical resistance | Good against oils, greases and fuels | Attacked by ketones, strong acids and some solvents. |
| Flammability | UL 94 HB | Standard grades. |
Typical room-temperature values for molded TPU of around Shore 95A. Printed TPU differs strongly by process: FDM parts depend on infill and layer bonding, and powder-bed (MJF) parts have markedly lower tensile strength and elongation than molded material. Use the data sheet of the grade or powder named in your quote, and test printed parts under the real load.
MJF printing TPU
MJF prints TPU without supports, which makes it the strongest option for complex flexible parts: cushioning lattices, bellows, integrated grips and soft-touch covers. Uretyco's MJF/SLS design guide was written around PA12; apply its rules with adjustments for flexible parts:
- Walls: treat 0.8 mm as cosmetic only and 1.5 mm as the functional minimum. Thin TPU walls are very floppy, so set stiffness with wall thickness and lattice cell size.
- Escape holes: hollows and closed lattices need powder escape holes, at least 4 mm and 6–8 mm for internal volumes above 50 cm³; fine flexible lattices are harder to depowder than rigid ones.
- Clearances: keep at least 0.5 mm between parts printed together; flexible assemblies may need more to separate cleanly.
- Surface: as-printed MJF TPU is grey and slightly grainy. Dyeing and vapor smoothing are listed among MJF finishes; confirm their availability for TPU in the quote.
FDM printing TPU
FDM is the low-cost route for flexible prototypes, bumpers, feet and simple gaskets. TPU 95A is the most printable of the flexible filaments, but it prints slowly and does not tolerate long unsupported bridges. Stiffness can be tuned with wall count and infill, so state whether parts should be solid or infilled. Tear resistance across layers is lower than along them, so orient straps and lips to flex along the layers. Uretyco's 3D printing guide advises testing fits and validating load-bearing printed parts under real conditions.
Injection molding TPU
For volume, TPU molds into tough, consistent parts with molded-in textures and is widely used for overmolding onto rigid substrates. The resin must be dried carefully before molding. Uretyco's DFM rules apply: keep walls uniform within about 25% and in the general 1.5–3.5 mm range, give at least 1° draft per side on outside walls, and keep gates and weld lines away from sealing lips and flex zones. Because the parts are flexible, shallow undercuts can sometimes be stripped from the mold instead of needing slides; the mould maker decides this when designing the tool.
Tolerances and surface finish
Uretyco's MJF/SLS guide plans ±0.3 mm or ±0.3% per linear feature for powder-bed parts; flexible TPU parts also deform under measuring force, so define how critical dimensions are measured. FDM tolerances depend on printer, orientation and size, so test fits first. Molded parts follow DIN ISO 20457 (formerly DIN 16742) by default, with surface finish or texture defined on the drawing. Final values are confirmed in the quote and the order.
Finishing options
| Finish | What it adds | Notes for TPU |
|---|---|---|
| As-printed | Lowest cost | Grainy grey surface (MJF) or visible layer lines (FDM). |
| Dyeing (MJF) | Even black color | Hides build lines; MJF dyeing is typically +10–15%. Confirm availability for TPU. |
| Vapor smoothing (MJF) | Sealed, smoother surface | Better feel and cleanability; typically +15–30% on MJF. Confirm availability for TPU. |
| Mold texture | Grip, matte feel | Defined in the tool; textured faces need extra draft (≈ 1° per 0.025 mm of depth). |
Cost and lead-time drivers
TPU is usually more expensive than standard filaments and prints more slowly, but the process choice dominates cost:
- MJF: priced by powder volume and build height, like PA12; hollows and lattices reduce cost, and build packing affects when parts ship.
- FDM: slow print speeds for flexible filament make print time the main driver; solid parts cost more than infilled ones.
- Molding: for runs under about 10,000 parts, aluminum tooling is typically 50–65% cheaper than steel and ships in 2–3 weeks.
- Documents: inspection reports and material documentation are opt-in and can extend the lead time. Request them at quote time.
TPU 95A vs. common alternatives
| Material | Hardness | Temperature range | Abrasion | Sealing / compression set | Processes on Uretyco |
|---|---|---|---|---|---|
| TPU 95A | Shore 95A | ≈ −30 to +80 °C | Excellent | Moderate | MJF, FDM, injection molding |
| Silicone (LSR) | Shore 10–80A | ≈ −60 to +200 °C | Fair | Low set; very good for seals | Injection molding, silicone molding |
| Cast polyurethane | Shore 30A–80D | Similar to TPU | Good | Moderate | Casting, silicone molding |
| PA11 | Rigid; flexes in thin sections | ≈ 80–100 °C | Good | Not a sealing material | SLS, MJF |
Use silicone for seals that see heat, cold or long-term compression, and TPU where abrasion, tear resistance and toughness matter more. Cast polyurethane covers small batches across a wide hardness range; PA11 suits living hinges and snap-fits rather than rubber-like parts.
When not to choose TPU 95A
Static seals under long-term compression, especially when warm: use silicone or a molded rubber. Service above about 80 °C or steam: use silicone. Precision parts or tight fits: flexible parts deflect under load and measurement. Hot, wet environments with polyester-based TPU: specify a polyether grade. Contact with ketones or strong acids.
Typical applications
- Grips, handles and soft-touch overmolds.
- Bumpers, feet, buffers and protective covers.
- Cushioning and energy-absorbing lattices (MJF).
- Cable strain reliefs, grommets and bellows.
- Gaskets and seals with modest compression demands.
- Wearables, straps and footwear components.
Specifying TPU 95A on Uretyco
- 1Choose the process
MJF for complex or lattice parts and small series, FDM for low-cost prototypes, injection molding for volume and overmolding.
- 2State hardness and grade
TPU 95A is the default; note softer hardness, a polyether type or food-contact needs in the order notes so availability is confirmed.
- 3Describe the load case
Note compression, stretching, abrasion, temperature and chemicals so the assistant can flag mismatches.
- 4Upload files and notes
STL or 3MF for printing (state solid or infilled for FDM); STEP and a drawing with parting line and gate preference for molding.
FAQ
What does Shore 95A feel like?
Firm, close to a hard rubber such as a shoe heel. Thin sections bend by hand, thick ones hold their shape. For softer parts, ask for a lower Shore grade; on printed parts, softness can also be tuned with wall thickness, infill or lattice design.
Can TPU be used for gaskets and seals?
For low-pressure, moderate-temperature seals and covers, yes. Because TPU takes a set under sustained compression, especially when warm, silicone or molded rubber is better for long-term static seals. Validate printed seals for leak-tightness; vapor-smoothed MJF surfaces seal better than as-printed ones.
MJF or FDM for TPU parts?
MJF suits complex geometry, lattices and small series, with consistent parts and no supports. FDM is cheaper for simple prototypes, feet and bumpers, and allows stiffness to be tuned with infill. When a part is feasible in both, Uretyco's quoting engine can compare them.
Related resources
- Liquid Silicone Rubber (LSR)For seals, heat and long-term compression.
- Cast PolyurethaneSmall batches across a wide hardness range.
- PA12 (Nylon 12)Rigid powder-bed parts that pair with TPU.
- Designing for MJF and SLSWalls, escape holes, fits and finishes.
- 3D PrintingChoosing between FDM, SLA, SLS and MJF.
- Injection Molding DFMWalls, draft, ribs, gates and tooling.
- Silicone MoldingSoft elastomer tooling paths.
- Material Selection GuideStart from the requirement, not the material name.
Related materials
Can't find what you need? Contact our team for expert assistance with your manufacturing project.