Uretyco
Make it now

Silicone Molding

Silicone molding on Uretyco: LSR injection molding, RTV silicone tooling with cast urethane parts, and compression molding. How each route works, when to choose it, design rules, materials, cost and lead-time drivers, and comparison with TPU and thermoplastic molding.

Overview

Silicone molding covers several routes to flexible, rubber-like parts and to low-volume parts that look and feel molded: liquid silicone rubber (LSR) injected into heated metal molds, RTV silicone molds used to cast polyurethane or silicone parts in small batches, and compression molding of solid silicone for gaskets and seals. Each route balances tool cost, surface detail, repeatability, and material properties differently.

LSR is a two-part, platinum-cured elastomer that is injected at low temperature into a hot tool, where it cures. Standard LSR grades cover roughly Shore 10A to 80A and a service range of about −60 to +200 °C, which makes silicone the default for seals, gaskets, membranes, and medical or food-contact parts.

How the three routes work

RouteHow it worksTypical use
LSR injection moldingThe two components are metered, mixed, and injected into a heated metal mold, where the silicone cures in the cavity; parts are demolded and deflashed where needed.Production seals, membranes, keypads, medical and food-contact parts
RTV silicone tooling (vacuum casting)A master model, often 3D-printed or machined, is cast in room-temperature-vulcanizing silicone to make a soft mold; polyurethane or silicone parts are then cast into it, usually under vacuum.Prototypes and bridge runs; parts that look and feel molded
Compression moldingA pre-weighed charge of solid silicone is placed in a heated mold and pressed until it cures.Gaskets, O-rings, and simple seals

When to choose

  • Elastic sealing, damping, or flexibility that must hold over wide temperature swings.
  • Medical or food-contact parts that need platinum-cured grades; confirm the exact grade and its documentation for your application.
  • Bridge quantities before hard tooling: cast urethane in silicone molds covers runs of up to about 200 parts.
  • Thin membranes, keypad webs, and intricate shut-offs that make use of silicone's stretch.

When not to choose

  • Rigid parts at production volume: thermoplastic injection molding gives a lower part price.
  • Parts exposed to heavy abrasion, where TPU or polyurethane usually performs better.
  • Large volumes of cast urethane parts: silicone molds wear out after a limited number of casts, so the part price stays high.
  • Tight dimensional tolerances on soft features: elastomers deform when measured, so define function-based acceptance instead.

Required files

FileUseNotes
STEP/STPPart geometryRequired. For RTV tooling, the master model is made from it.
PDF drawingShore hardness, material grade, color, critical dimensions, parting-line and gate preferences, cosmetic facesStrongly recommended before tooling.
Reference sampleHardness feel, color, textureUseful when matching an existing part.

Design rules

  • Specify Shore hardness and, where it matters, tear strength: silicone stiffness spans an enormous range.
  • Avoid sharp internal corners; generous radii reduce tearing during demolding.
  • Keep walls as uniform as practical; thick sections take longer to cure.
  • LSR flows very easily and can flash at tool splits: map cosmetic surfaces relative to parting lines and gate vestiges.
  • Moderate undercuts can often be stripped from the mold because silicone stretches; confirm with the supplier before relying on it.
  • Validate shrinkage separately from thermoplastics; silicone behaves differently from thermoplastic melts.
  • For overmolding onto plastic or metal, agree the substrate and bonding method (self-bonding grade or primer) with the supplier.

Typical materials

MaterialHardnessTypical useNotes
Liquid silicone rubber (LSR)Shore 10A–80ASeals, gaskets, membranes, medical and food-contact partsAbout −60 to +200 °C; tensile strength ≈ 5–11 MPa, elongation 200–700%
Solid silicone for compression moldingWide rangeGaskets, O-rings, simple sealsLower tool cost than LSR, more manual handling
Cast polyurethaneShore 30A–80DLook-alike parts for ABS, PC, or rubber; grips, bumpers, housingsCast in silicone molds; from soft elastomer to rigid plastic
TPU 95A (alternative)Shore 95AAbrasion-resistant flexible parts, printed (MJF) or injection moldedService temperature up to about 80 °C

Tolerance expectations

Tolerances for silicone parts are confirmed per part in the quote rather than taken from a general tolerance class. Soft parts deform under measuring force, so define how a critical dimension is measured, for example a seal cross-section or its compression, and base acceptance on function wherever possible.

RequirementTypical guidanceCost impact
Seal cross-section and compressionState the nominal value and how it is measured; validate with a functional testMedium
HardnessGive a Shore A target with a tolerance bandLow
Cosmetic surfacesMap flash lines, gate vestiges, and textureMedium
Overmolded or bonded featuresDefine the substrate, bond requirement, and testMedium to high
Quote-dependent values

Tolerance, finish, material, inspection, and lead-time values are practical guidance. Binding values are those confirmed in your quote and order, based on the material, drawing and production method.

Cost drivers

  • Tooling route: a machined, heated LSR mold costs far more than an RTV silicone mold but lasts for production volumes; RTV molds wear out after a limited number of casts.
  • Material grade: medical, food-contact, flame-retardant, or color-matched grades cost more than standard ones.
  • Hardness, color, part size, and cure time for thick sections.
  • Deflashing, post-curing, and secondary bonding or assembly.
  • Inspection and documentation: first articles, functional tests, and material certificates on request.

Lead-time drivers

  • RTV silicone tooling with cast urethane parts: typically 1–2 weeks to first parts, according to Uretyco's bridge-production guide.
  • LSR needs a machined metal mold, so, as with thermoplastic injection molding, tool manufacture and sampling dominate the first delivery.
  • Special grades, custom colors, post-curing, and documentation add time.

Silicone molding versus alternatives

OptionBest forToolingNotes
LSR injection moldingProduction volumes of seals, membranes, medical and food-contact partsMachined, heated metal moldTighter repeatability than RTV; high tool cost
RTV silicone mold with cast urethanePrototypes and bridge runs of up to about 200 partsLow-cost silicone mold made from a master1–2 weeks to first parts; limited mold life
Compression moldingGaskets and simple sealsSimple heated moldLower tool cost than LSR; more manual handling and flash
TPU, printed (MJF) or injection moldedAbrasion-resistant flexible partsNone for printing; mold for injection moldingMuch lower temperature resistance than silicone
Thermoplastic injection moldingRigid parts at volumeAluminum or steel moldSee the injection molding guide

Uretyco AI workflow

  1. 1
    Use-case questions

    The assistant asks about the sealing function, temperature, chemicals, skin, food, or medical contact, hardness, and quantity.

  2. 2
    Route comparison

    LSR, RTV casting, compression molding, and TPU are compared on tool cost, unit price, and lead time; silicone can also be compared with thermoplastic injection molding.

  3. 3
    Material and documentation

    Grade, hardness, color, and any certificates are fixed in the order scope; certificates are provided on request.

  4. 4
    Sampling and production

    First articles are checked before the full run; parts are then molded or cast, deflashed, inspected, and packed.

Quality notes

  • Give hardness as a Shore A value and define color with a reference sample.
  • Mark cosmetic faces and where flash lines and gate marks are acceptable.
  • State medical or food-contact use before quoting; suitability for the final application remains your responsibility.

FAQ

LSR or RTV?

LSR suits higher volumes and tighter repeatability. RTV silicone molds suit prototypes and low volumes, with first parts in about 1–2 weeks.

Can silicone replace TPU?

Sometimes, mainly for temperature or chemical resistance: LSR is rated from about −60 to +200 °C, while TPU 95A is limited to about 80 °C. TPU resists abrasion better and damps differently, so test the part in its real environment.

Can I get food-contact or medical-grade silicone?

LSR grades for food contact and for medical use (tested to ISO 10993) exist. State the requirement before quoting: the exact grade and its documentation are fixed in the order scope, certificates are provided on request, and whether the final part is suitable for your application remains your responsibility.

Does Uretyco compare silicone with injection molding?

Yes, based on quantity, tolerance, material needs, and cosmetic goals.

Was this page helpful?

Can't find what you need? Contact our team for expert assistance with your manufacturing project.

Contact our team