Overview
Die casting forces molten non-ferrous metal (zinc, aluminum, or magnesium alloys) into a hardened steel die under high pressure. The metal solidifies quickly, the die opens, and the casting is ejected with thin walls, ribs, bosses, and mounting features already formed. Because the shape comes from the die, parts repeat closely and need far less material removal than parts machined from solid stock.
Like injection molding, die casting trades a significant up-front die cost for a low price per part. It is the right choice at moderate to high volumes once the design is stable; for prototypes and low volumes, CNC machining is usually faster and cheaper.
How it works
- 1Die design and DFM review
Draft, wall thickness, radii, parting line, gate and overflow positions, and ejector locations are defined; undercuts are designed out or given slides.
- 2Die manufacturing
The die halves are machined from hardened tool steel, with cooling channels, cores, and any slides.
- 3Casting
Zinc alloys run on hot-chamber machines; aluminum alloys run on cold-chamber machines, where metal is ladled into a shot sleeve for every shot. Magnesium can run on either, depending on part size.
- 4Trimming and secondary operations
Runners, overflows, and flash are trimmed off; critical features are machined, and the parts are finished, inspected, and packed.
When to choose
- Moderate to high volumes, where the die cost is spread over enough parts to beat machining from bar or plate.
- Thin walls, ribs, bosses, and mounting features integrated into one casting instead of a welded or bolted assembly.
- Housings, heat sinks, connectors, brackets, and enclosures in zinc, aluminum, or magnesium alloys.
- Cosmetic metal parts, provided flash removal and the finishing plan are defined up front.
When not to choose
- Prototypes and design iterations: machine the part until the design is stable.
- Steel or stainless steel parts: die casting is limited to non-ferrous alloys.
- Parts that must be welded or solution heat-treated (T6) after casting, unless alloy and process are chosen for it.
- Pressure-tight or highly stressed parts without a defined porosity acceptance and test plan.
- Very thick, solid sections: they trap porosity and lengthen the cycle; core them out or choose another process.
Required files
| File | Use | Notes |
|---|---|---|
| STEP/STP | Cast geometry, including draft | Required for die design and DFM analysis. |
| PDF drawing | Alloy, tolerances, machined features and allowances, datum scheme, finish, porosity or leak-test requirements | Strongly recommended before the die is cut. |
| Reference sample | Cosmetic or fit benchmark | Useful when matching an existing part. |
Design rules
- Keep walls as uniform as possible and change thickness gradually; thick sections and abrupt transitions are where porosity forms.
- Core out heavy sections and add ribs for stiffness instead of mass.
- Add draft to all surfaces parallel to the die opening. Inner walls and cores need more draft than outer walls, because the metal shrinks onto them as it cools.
- Use generous fillets and radii at every junction; sharp corners disturb metal flow, concentrate stress, and shorten die life.
- Avoid undercuts where possible; each one needs a slide, which adds die cost and maintenance.
- Define the parting line and the gate, overflow, and ejector-pin locations relative to cosmetic and sealing faces.
- Avoid tight dimensions across the parting line or moving slides; they vary more than dimensions within one die half.
- Add a machining allowance and a clear datum scheme for every feature that will be machined after casting.
Typical alloys
| Alloy family | Common examples | Typical reason to choose |
|---|---|---|
| Zinc | Zamak 3, Zamak 5 | Fills thin walls and fine detail well, is a good base for plating, and gives long die life because it casts at a lower temperature; dense, so best for smaller parts. |
| Aluminum | A380, ADC12, EN AC-46000 (AlSi9Cu3) | Light and strong for structural housings, enclosures, and heat sinks; the most widely used die-casting family. |
| Magnesium | AZ91D | Lightest structural metal; thin-walled housings where weight matters most. |
Aluminum A356 is a sand, investment, and permanent-mold casting alloy that is usually heat-treated to T6; it is not a typical high-pressure die-casting alloy. If you need A356-type properties, say so in the order notes, which go to the manufacturing partner with the part.
Porosity and process risks
The die fills in a fraction of a second, so trapped air and shrinkage can leave small voids (porosity), mostly in thick sections and at abrupt wall transitions. Some porosity is normal in die castings; it matters most for pressure-tight parts and for surfaces that will be machined, because machining can open pores below the dense outer skin.
- Design for uniform walls and agree on gate, venting, and overflow positions with the supplier; vacuum-assisted casting reduces gas porosity where it is available.
- For pressure-tight parts, state the leak-test requirement and the porosity acceptance on the drawing; impregnation can seal porosity after machining.
- Conventional die castings are usually not solution heat-treated or welded, because entrapped gas can cause blistering. Confirm mechanical targets against the supplier's alloy data.
- Keep machining allowances small on surfaces where the dense outer skin matters.
Secondary operations and finishing
Critical sealing surfaces, bearing bores, and datum features often receive light machining after casting, so include machining allowances and datum schemes on the drawing. Other common steps are trimming, deburring or vibratory finishing, tapping, impregnation, and surface finishing.
| Finish | Notes for die castings |
|---|---|
| Powder coating or painting | Common for aluminum and zinc housings. Needs a clean, pretreated surface; gas escaping from porosity during curing can cause defects, so mention it if parts will be coated. |
| Plating (e.g. nickel, chrome) | Zinc die castings are a classic base for decorative plating; surface quality before plating decides the result. |
| Anodizing | Possible on die-cast aluminum, but high-silicon die-casting alloys anodize unevenly and gray; for cosmetic anodizing, machined 6061 is more consistent. |
| Chromate conversion coating | Corrosion protection and paint base with negligible build-up; the surface stays electrically conductive. |
Tolerance expectations
As-cast tolerance depends on the alloy, the part size, and whether a dimension lies within one die half or crosses the parting line or a slide. Die-casting tolerances are confirmed per part in the quote: specify critical dimensions on the drawing and plan machining for fits, bores, and sealing faces.
| Requirement | Typical guidance | Cost impact |
|---|---|---|
| Dimensions within one die half | As cast, per drawing and supplier capability | Low |
| Dimensions across the parting line or slides | Allow more variation, or machine after casting | Medium |
| Bores, fits, sealing faces | Machine after casting; specify allowance and datums | Medium to high |
| Pressure tightness | Define leak test and porosity acceptance; impregnate if needed | Medium to high |
Tolerance, finish, material, inspection, and lead-time values are practical guidance. Binding values are those confirmed in your quote and order, based on the material, drawing and production method.
Cost drivers
- The die: size, number of cavities, slides for undercuts, cooling, and steel grade. It is a significant one-time cost, so quantity decides whether die casting pays off.
- The part: alloy, part weight, the machine size needed for the projected area, and cycle time.
- Trimming, deburring, machining, tapping, and impregnation after casting.
- Finishing, masking, and cosmetic acceptance criteria.
- Inspection: first-article reports, CMM measurement, leak testing, or X-ray inspection where porosity matters.
Lead-time drivers
- Die design, manufacture, and sampling dominate the first delivery; repeat orders on an existing die mainly wait for the production queue.
- First-article approval and any die corrections happen before production is released.
- Machining, impregnation, and finishing are separate operations that add time after casting.
- Inspection reports and material documentation are opt-in and add time; request them at quote time.
Die casting versus alternatives
| Process | Best for | Tooling | Unit cost at volume | Notes |
|---|---|---|---|---|
| Die casting | Moderate to high volumes of thin-walled non-ferrous parts | Hardened steel die, high cost | Low | Near-net shape; porosity must be managed |
| CNC machining | Prototypes, low volumes, tight tolerances | None | High | Best dimensional control; any machinable metal |
| Sand casting | Low volumes, large or heavy parts | Pattern, low cost | Medium | Rougher surface, thicker walls, more machining |
| Investment casting | Complex shapes; wider alloy range including steels | Wax-pattern tooling, medium cost | Medium | Good surface and detail; slower cycle |
| Sheet metal fabrication | Brackets, panels, and enclosures from flat stock | Little or none | Low to medium | Limited to formed sheet geometry |
Upload the model and describe quantity and function: the quote engine scores casting alongside CNC machining and sheet metal, and the assistant can explain the tradeoff for your part.
Uretyco AI workflow
- 1Geometry analysis
Uretyco checks wall thickness, thick sections, draft, undercuts, and features that will need machining.
- 2Volume and alloy questions
The assistant asks about annual quantity, alloy, pressure tightness, finish, and which features are critical.
- 3Process comparison
Die casting is compared with machining and other routes on die cost, unit price, and lead time.
- 4First article and production
Initial castings are reviewed before the full run; parts are then cast, trimmed, machined, finished, and inspected to the agreed scope.
Quality notes
- Mark the sealing faces, bores, and datum features that will be machined, and state the allowances.
- Define porosity acceptance and any leak or pressure test for fluid-carrying parts.
- Request first-article approval before the full run. Material certificates are opt-in: ask for them at quote time if you need them.
- Mark cosmetic surfaces and acceptable locations for parting-line, gate, and ejector marks.
FAQ
Zinc or aluminum?
Zinc fills thin walls and fine detail best, plates well, and gives long die life, but it is about two and a half times as dense as aluminum, so it suits smaller parts. Aluminum is the choice for lightweight structural housings and heat sinks; magnesium when weight is critical.
Can die castings be heat-treated or welded?
Conventional high-pressure die castings usually are not solution heat-treated or welded, because gas trapped in the casting expands and causes blisters. If the part needs T6 properties or welding, choose an alloy and process that allow it; the DFM findings show how well the part suits the process.
Is A356 a die-casting alloy?
Not typically. A356 is used for sand, investment, and permanent-mold castings and is usually heat-treated to T6. Typical high-pressure die-casting alloys are A380, ADC12, or EN AC-46000 for aluminum and Zamak 3 or Zamak 5 for zinc.
When is CNC machining the better choice?
When quantities are low, the design is still changing, or many features need tight tolerances. Machining needs no die and gives the best dimensional control, and cast parts often need machining on their critical features anyway.
Related resources
- Molding & Casting OverviewCompare molding and casting processes.
- CNC MachiningThe no-tooling alternative for low volumes.
- Aluminum A356 (Cast)Cast aluminum for sand, investment, and permanent-mold casting.
- Surface FinishingCoatings, masking, and dimensional effects.
- Quality Control & InspectionFirst articles, reports, and certificates.
- Technical Drawings & TolerancesDatums, allowances, and critical dimensions.
- Choosing the Right ProcessCompare all processes.