Uretyco
Make it now
Stainless Steel 304 (A2 / 1.4301)

Stainless Steel 304 (A2 / 1.4301)

Metals
Stainless304AusteniticFood-grade

Stainless steel 304 (1.4301 / A2) reference: typical properties, CNC machining notes, passivation and finishing options, cost drivers, and comparison with 303, 316L, 17-4 PH and 6061.

Stainless steel 304 (EN 1.4301, X5CrNi18-10, also called A2 or 18/8) is an austenitic chromium-nickel steel with about 18% chromium and 8–10.5% nickel. It is the default stainless: excellent corrosion resistance in air, fresh water and most food and cleaning environments, high toughness down to cryogenic temperatures, and no coating required.

Choose it when a machined part must stay clean and rust-free without a finish: food and beverage equipment, laboratory and medical device hardware, enclosures and fittings. Its limits are chloride environments (seawater, de-icing salt, swimming pools), where 316L is the safer choice, and machinability: 304 work-hardens, so it machines more slowly than aluminum or mild steel. Besides CNC milling and turning, 304 can be ordered through Uretyco for sheet metal and casting.

Mechanical and physical properties

PropertyTypical valueNotes
Tensile strength (Rm)515–700 MPaMinimum 515 MPa (ASTM A240); EN 10088 range ≈ 500–700 MPa, by product form.
Yield strength (Rp0.2)≥ 205 MPaEN 10088 minimums ≈ 190–230 MPa by form; annealed bar is typically ≈ 215–300 MPa, cold-drawn bar higher. Lower than 6061-T6 (276 MPa).
Elongation at break≥ 40%Typically 50–60%; very ductile and tough.
Hardness≈ 150–200 HBASTM A240 maximum 201 HB (92 HRB) annealed; the cut surface work-hardens.
Elastic modulus193 GPaAbout 2.8× aluminum.
Density7.9–8.0 g/cm³≈ 3× aluminum.
Thermal conductivity16.2 W/m·K≈ one-tenth of 6061; heat stays at the cutting edge.
Thermal expansion17.3 µm/m·KAbout 1.5× carbon steel; matters in steel/stainless assemblies.
Magnetic behaviorNon-magnetic when annealedBecomes slightly magnetic after cold work and machining.
Pitting resistance (PREN)≈ 18–20316L: ≈ 23–26.
Service temperatureCryogenic to ≈ 870 °C in airOxidation limit for intermittent use; avoid long holds at 425–860 °C where corrosion matters (sensitization; use 304L).
Typical values, not design allowables

Typical room-temperature values for annealed wrought 304; strength depends strongly on cold work, so cold-drawn bar can be much stronger than plate. For calculations, use the minimums of the governing standard (e.g. ASTM A240/A276, EN 10088-2/-3) or your material certificate.

Machining 304 stainless

304 is gummy and work-hardens quickly: a tool that rubs instead of cutting leaves a hardened skin that makes the next pass harder. Low thermal conductivity concentrates heat at the cutting edge. Rigid setups, sharp coated carbide, moderate cutting speeds, a steady feed and plenty of coolant matter far more than on aluminum. Watch for:

  • Work hardening: avoid dwelling, light finishing passes that rub, and peck cycles that re-cut the hardened bottom of a hole. Keep the tool engaged and the chip load constant.
  • Thin walls: the CNC Design Guide sets 1.2 mm as the practical minimum for stainless 304, with pocket depth up to about 3× the opening, stricter than the 0.8 mm and 4:1 used for aluminum.
  • Chips and burrs: turning produces long, stringy chips that need chip breakers, and burrs are tough. Specify an edge break where burrs matter; Uretyco's default is light deburring.
  • Threads: use standard sizes (M2–M10), 1.5–3× the diameter deep. Stainless screws in stainless threads can gall (cold-weld) and seize; use anti-seize, a different fastener material or thread inserts on parts assembled repeatedly.
  • Free-machining 303: for turned parts in volume, 303 (1.4305) cuts much faster thanks to added sulfur, at the cost of lower corrosion resistance and poor weldability. Note it in the order if it is acceptable.

Tolerances and surface finish

Uretyco treats unspecified tolerances as ISO 2768-mK, with a default as-machined surface of around Ra 1.6–3.2 µm and light deburring. Tighter tolerances, finer Ra values and fits need a 2D drawing and belong on functional features only. Each tight tolerance costs more machine time in 304 than the same callout in aluminum, so keep them to mating features. Final values are confirmed in the quote and the order.

Finishing options

304 needs no coating to resist corrosion, so finishing is mainly about cleanliness, appearance and restoring the passive layer after machining. Iron particles picked up from tools, fixtures or steel blasting media can rust on the surface and make the part look as if it is corroding.

FinishWhat it addsNotes for 304
As-machinedLowest costClean, bright metal with visible tool marks; fine for most internal parts.
PassivationRestores the passive layerAcid treatment per ASTM A967 removes free iron; no dimensional change. Specify it for parts in corrosive or hygienic service.
Bead blastUniform matte lookUse glass or ceramic media, not steel shot; usually followed by passivation.
BrushedUniform directional grainCommon on visible faces; define the grain direction on the drawing.
ElectropolishSmooth, bright, cleanable surfaceRemoves a few micrometers and levels micro-peaks; improves cleanability and corrosion resistance. State the target Ra.
Mirror polishOptical or sealing surfacesRa below ≈ 0.4 µm; one of the most expensive finishes.
Specify passivation explicitly

Passivation is not automatic. If the part goes into wet, food or medical service, write the requirement on the drawing (for example "passivate per ASTM A967") and keep steel tools, steel wire brushes and steel media away from stainless surfaces.

Cost and lead-time drivers

As a rule of thumb, material is typically 10–30% of a CNC quote, machine time 35–55% and finishing 0–25%. For 304, machine time is the main lever: slower cutting and faster tool wear make the same geometry noticeably more expensive than in aluminum. The main levers:

  • Geometry: thicker walls, larger internal radii and shallower pockets save more cutting time in stainless than in aluminum.
  • Setups: a part machined in two setups costs roughly half of one that needs four.
  • Stock and grade: 304 is widely stocked; Uretyco's stainless comparison puts 316L at about 1.4× and 17-4 PH at about 1.6× the cost of 304. Stock material is usually faster than a special order.
  • Finishing and documents: bead blast typically adds 5–10% and mirror polish 50–150%. Material certificates and inspection reports are opt-in and can extend the lead time; request them at quote time.

304 vs. common alternatives

MaterialStrengthMachinabilityCorrosionWeldabilityRelative cost
304Baseline (Rm ≥ 515 MPa, Rp ≥ 205 MPa)Fair; work-hardensVery good indoors and in fresh waterExcellent (304L for welded parts)Baseline
303SimilarGood; free-machiningLower than 304PoorSimilar stock, faster machining
316LSlightly lower (Rm ≥ 485 MPa)Fair; gummier than 304Better; resists chloridesExcellent≈ 1.4×
17-4 PH≈ 2× or more (Rm ≈ 1000–1300 MPa, by condition)FairGood, below 316LGood, with post-weld heat treatment≈ 1.6×
6061-T6 + anodizeLower Rm (≈ 310 MPa), higher yield (276 MPa)GoodGoodGood; weld zone softensLower

If weight matters more than corrosion resistance, anodized 6061-T6 weighs a third as much and machines far faster; if strength matters, 17-4 PH reaches roughly five times the yield strength of annealed 304. Wherever chlorides are present, choose 316L instead of 304.

When not to choose 304

Common mismatches

Seawater, splash zones, de-icing salt, swimming pools or chloride cleaners: 304 suffers pitting and crevice corrosion; use 316L. Welded assemblies in corrosive service: specify 304L to avoid sensitization. High strength, hardness or wear resistance: 304 cannot be hardened by heat treatment; consider 17-4 PH or 4140. Weight-critical parts: consider 6061-T6 or 7075-T6. High-volume turned parts where machining cost dominates and corrosion demands are mild: consider 303.

Typical applications

  • Food, beverage and dairy processing components.
  • Laboratory, pharmaceutical and medical device hardware (non-implant).
  • Enclosures, panels and fittings for indoor and fresh-water environments.
  • Shafts, pins, bushings and spacers that must not rust.
  • Valve, pump and fluid-handling parts for water and mild chemicals.
  • Architectural and consumer hardware with brushed or polished finishes.

Specifying 304 on Uretyco

  1. 1
    Select 304 and a finish

    Add passivation for wet, food or medical service; note 304L for welded parts and 303 if a free-machining grade is acceptable.

  2. 2
    Upload STEP plus a 2D drawing

    Needed for anything tighter than ISO 2768-mK, threads, Ra, grain direction or GD&T.

  3. 3
    Request documents at quote time

    Material certificates and inspection reports are opt-in; ask for them before production, not after shipment.

FAQ

What is the difference between 304 and 304L?

304L (1.4307) has a maximum carbon content of 0.03% instead of 0.07–0.08%, so it does not sensitize during welding. It is slightly weaker on paper. Many mills supply dual-certified 304/304L, but state 304L on the drawing if the part will be welded.

Is 304 magnetic?

Annealed 304 is essentially non-magnetic. Cold working and machining can transform part of the surface structure, so machined or bent 304 parts may be slightly attracted to a magnet. This does not mean the material is wrong. If low magnetic permeability is a requirement, state it and consider 316L, whose structure is more stable.

Is 304 food-safe?

304 is one of the most widely used stainless steels in food and beverage equipment. Food-contact suitability, however, also depends on surface finish, cleanability and the regulations in your market, so state the intended use and any required finish (for example passivation or electropolishing) in the order. Material certificates can be requested at quote time.

What do A2, 1.4301 and 18/8 mean?

All three describe the same family. 1.4301 (X5CrNi18-10) is the EN material number, A2 is the stainless designation used for fasteners (ISO 3506), and 18/8 refers to the nominal chromium and nickel content. AISI/ASTM 304 and EN 1.4301 are close equivalents, not identical, so confirm substitutions on certified parts.

Related materials

Was this page helpful?

Can't find what you need? Contact our team for expert assistance with your manufacturing project.

Contact our team